Rapier
Senior Member
Hand lapping a rifle barrel is a PIA. First you need a rod with a bearing handle that will turn freely, plus a patch style loop at the end. Pour molten hard casting lead around the loop end so the loop holds the lead plug inside the barrel. Pull the lead plug half way out (do not pull the plug totally out of the lands at any point in this process) apply your courses grinding compound then push the plug half way out of the other end, apply compound, draw the plug half way out and repeat until the bore feels smoother, pull the plug half way out, wipe clean and apply finer compound, push back until half way out, wipe and apply the fine compound, repeat with finer compound until the bore is smooth and shiny. At any point if you pull or push the plug out all the way, you must restart from pouring the lead.
Fire lapping, use 5 hard cast bullets lubed with the grit of choice, fire at low velocity, patch the bore, examine closely, repeat as necessary until you get the desired result. I use an 800 grit finish for cast bullet bores. I have removed milling marks from lands and chatter marks from grooves using fire lapping. Fire lapping is a ton easier method.
You can fire lap a 22 LR barrel by cutting grooves around the bullet with a motor tool and a fine saw blade then lube the bullets with very fine grit. Some polish a 22LR bore with pine rosin (rimfire BR) on the 22 bullet with cut grooves as the end polish.
A bumble bee can fly faster than a tractor.